ASTM A106 pipe is always produced by the seamless method and can be bent, coiled and flanged.
Sizes
1†– 26†dependent on OD vs Wall Ratio
Process
The steel shall be killed steel, with the primary meltling process being open-hearth,basic-oxygen,or electric-furnace,possibly combined with separate degassing or refining. If secondary melting, using electroslag remelting or vacuum-arc remelting is subsequently employed, the heat shall be defined as all of the ingots remelted from a single primary heat.