PHYSICAL PROPERTIES Specific Heat: BTU/lb-°F (J/g-°K): 0.110 (460) Mean Coefficient of Thermal Expansion: µin/in-°F (µm/m-°C) 70 - 200 °F (20 - 95 °C): 7.4(13.3) Density: 0.322 lb/in3, 8.91 g/cm3Electrical Resistivity: ohm-cir-mil/ft,(µohm•m): 45.0 (0.075) PROPERTIES: TEMPEREDNickel 270 can be cold worked to various tempers. Contact ASHAPURA STEEL for additional information.